Tim Oster wrote:
>
> To Scott:
>
> Board houses do not like to route through copper when they cut out the boards. G10 is pretty bad on cutters as it is, when you introduce copper into the problem things tend to wearout VERY quickly.
>
> Timo
Yes, that's unfortunate, but if you do need the copper to the edge
of the PCB (i.e. for shielding purposes) then there's no way
around it, right?
Regards
Eric Bonatti
<< UBI MAJOR, MINOR CESSAT >>
----------------------------------------------------------------
Eric Bonatti - Printed Circuit Board Design
GN Nettest (CANADA) Datacom Division
phone: 905-479-8090 xt.497 / fax: 905-475-6524
email: [log in to unmask]
web: http://www.nettestca.gn.com
----------------------------------------------------------------
"...now I'm singing all my songs to the girl who won my heart,
she is only three years old and it's a real fine way to start!"
(The Ocean, Led Zeppelin)
##############################################################
IPC Designers Council Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DESIGNERCOUNCIL <your full name>
To unsubscribe: SIGNOFF DESIGNERCOUNCIL
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|