Technetters,
1) We are interested in tape as protection for gold connectors before
HAL.
Would someone please contact me with recommendation and past experience
on such kind of tape. (Is it applied and removed manually?, Should the
boards brushed after removing the tape?.
2) We are looking for special rubber (If there is such) to clean "dark
gold fingers"
Any feedback would be much appreciated
Tomer
##############################################################