I'm looking for a thermally conductive adhesive (silicone based or similar)
with the following properties:
Lap sheer strength ~700 psi
Thermal conductivity ~5 BTU in/hr-F-ft2 (~.008 watts/cm-C)
Consistency Paste
And most importantly... fungus resistant.
Any help will be appreciated.
Thanks
Jim Marsico
(516) 595-5879
[log in to unmask]
##############################################################