TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Shea, Daniel" <[log in to unmask]>
Reply To:
TechNet Mail Forum.
Date:
Fri, 12 Dec 1997 08:44:59 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (72 lines)
The material we have used in the past is Delmat or ECP-Plus for this
application.

A supplier of ECP-Plus is:

EMC Global Technologies
4059 Skyron Drive
Doylestown, PA 18901
Tel; 215-340-0650
Fax: 215-340-1737

We have used them successfully to design and fabricate the fixtures as
well.

Dan Shea
Sr. Manufacturing Engineer
The Foxboro Company
Tel #  508-549-2410
Fax # 508-549-4379
Email: [log in to unmask]


-----Original Message-----
From:   Blanchet,Richard [SMTP:[log in to unmask]]
Sent:   Thursday, December 11, 1997 5:20 PM
To:     [log in to unmask]
Subject:        [TN] Assy: Selective soldering

Hello,

I'd be interested in learning about anybody's experience with
selective
soldering done on a full-size wave soldering machine. I'd like to know
what
materials you guys use to cover the solder bath or the PCB itself, as
well
as things to pay special attention to, tricks, tips, etc.

You can respond to me through technet or directly. Thank you.

Richard Blanchet
Manufacturing Engineer
Canadian Marconi
[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2