I am looking for a lab to perform failure analysis (materials/surface
analysis) on mealed urethane conformal coat. The mealing of the coating on
our circuit card assemblies occurred during system-level humidity
qualification testing. Ideally the lab or analyst would have expertise in
urethane coatings failure mechanisms. All suggestions welcome. Thanks.
---
Gregg Klawson
GTE Government Systems Corp, Taunton, Massachusetts, USA
[log in to unmask], telephone +1.508.880.1822
The views expressed are the author's and do not necessarily reflect the
official position of GTE or any of its subsidiaries.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|