TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Ed Cosper <[log in to unmask]>
Date:
Mon, 22 Dec 1997 16:22:00 -0600
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Jerry Cupples <[log in to unmask]>
Subject:
From:
Jerry Cupples <[log in to unmask]>
In-Reply-To:
<01BD0EF2.3FC39A20@gateway>
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (49 lines)
Ed Cosper asked:

>What would a normal temperature range for wave solder be for a standard
>FR4 product and roughly how many seconds of exposure to the wave would be
>typical.

Trying to live up to Jack's high praise:

Eutectic tin-lead pot operating temp at ~ 470-500 degrees F is normal.

Your exposure is a function of the wave contact length, typically measured
with a tempered glass fixture. Contact length is perhaps 1-3 inches. This
sometimes changes without the operator knowing, due to the variation of the
solder pump head, pump speed, the thickness of the board, etc.

Conveyor settings of at 4-6 ft/min would then give you (check my math):

conveyor       contact time
setting      per inch of wave
-------      ----------------
4 fpm             1.25 sec
6 fpm             0.83 sec
8 fpm             0.62 sec

So, it could range from 3.75 seconds with the 4 fpm conveyor & 3" wave to
0.6 sec with an 8 fpm conveyor rate and a 1" wave. I'd say 2 seconds is
quite typical. YMMV.


cheers,


Jerry Cupples
Interphase Corporation
Dallas, TX USA
http://www.flash.net/~cupples

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2