Can someone in Technetland tell me how the acceleration factor of 1 week at
85C/85% RH equivalence to 1 year of tropical service was derived?
Also, what is the acceleration factor for the Class 2, 50 C, 80% RH
conditions?
Does anyone have a method for calculating acceleration factors for
conditions that deviate from those
above?