I have found when discussing this practice with those still using it is either because they are building press fit back panels, which panel plating provides a more consistent hole size, or because of the old - "well that's the way we've always done it. " I have found only a few that indicated the do it to prevent voids due to an apparent inadequate electroless process.
----------
From: [log in to unmask][SMTP:[log in to unmask]]
Sent: Wednesday, December 03, 1997 10:30 AM
To: [log in to unmask]
Subject: [TN] Plating
Why are so many plants doing panel plating or flash
plating as opposed to doing a heavy deposition and
then pattern plating ?
There is probably an easy answer that I cannot come
up with.
thanxx
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|