I am currently chemically engraving steel plates for printing. I am using
an electronic device to measure the etch depth to within +- 2 microns. This
device is made by a German co. called perthen, I am currently looking for
any other means of measuring etch depth to within Microns. Preferably a US
distributor.
----------
> From: Leon Snowdon <[log in to unmask]>
> To: [log in to unmask]
> Subject: Re: [TN] Supplier
> Date: Thursday, December 11, 1997 12:05 PM
>
> THE ADDRESS OF DRAEGER IS:-
>
> Draeger Ltd.,
> Kitty Brewster Estate,
> Blyth,
> Northumberland
> NE24 4RG
>
> The Tel. No. is :- 01670 352891 and FAX No. is:- 01670 361732
>
> Hope this helps.
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|