TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Tom Taylor <[log in to unmask]>
Date:
Thu, 4 Dec 1997 10:00:17 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Tom Taylor <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
>Getter is often referred to as fly paper that will catch loose
>particles during centrifuge testing
>
"Getter" is also the material placed in vacuum tubes to
remove the last traces of oxygen and other gases to
avoid reaction with the filament.

From an old electronics dictionary:

"An alkali metal introduced into a vacuum tube during
manufacture.  It is fired after the tube has been evacuated,
to react chemically with and eliminate any remaining gases.
The getter then remains inactive inside the tube.  The
silvery deposit sometimes seen on the inside of the glass
envelope is due to getter firing".

One source for these materials--which depend on the
application and the gases to be removed--is SAES Getters:

http://www.avem.org/SAES.html

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2