Almost sounds like crystallized water molecules, check the rinse tanks!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jana Carraway
Sent: Tuesday, December 23, 1997 1:15 PM
To: [log in to unmask]
Subject: Re: [TN] White residue
It must be a function of temperature of the process!
Jana
Nicholas Kane <[log in to unmask]> Wrote:
|
| Is this white residue on circuit boards the same stuff
| that everyone is
| talking about in Boston et al? Seems the people in Boston
| have got a very
| serious problem with their process if there is 12 inches
| of it.
|
| Perhaps it is a regional thing - never had this sort of
| problem in this
| region. Perhaps you'd better move all your plants over
| here.
| Nicholas Kane
| Axion Australasia
| Suite 3, 651 Canterbury Road
| Surrey Hills
| Victoria 3127 Australia
|
| ##########################################################
| ####
| TechNet Mail List provided as a free service by IPC using
| LISTSERV 1.8c
| ##########################################################
| ####
| To subscribe/unsubscribe, send a message to
| [log in to unmask] with following text in the body:
| To subscribe: SUBSCRIBE TECHNET <your full name>
| To unsubscribe: SIGNOFF TECHNET
| ##########################################################
| ####
| Please visit IPC web site
| (http://www.ipc.org/html/forum.htm) for additional
| information.
| For the technical support contact Dmitriy Sklyar at
| [log in to unmask] or 847-509-9700 ext.311
| ##########################################################
| ####
|
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|