In a message dated 12/17/97 14:01:17, you wrote:
>Engelmaier:
>Then how about plugging of the vias using epoxy, will it be less reliable or
>more reliable. Also fab house can't completely fill the via barrel using
>epoxy (may be 30% of the barrel will be filled) and they won't recommend
>filling of vias from both side as entrapped moisture can remove the plug
>from one side during thermal excursion. Also they can not fill all the vias
>- may be 90% vias will be covered.
>What you recommend from reliability point of view?
>re,
>ken patel
Hi Ken,
I am not aware of any study on this issue, and I have not done any either— so
all I can give you is a semi-educted guess. The epoxy is softer than solder
and because it does not wet solder will have a different geometry at the
filled/unfilled interface. Both of these facts make the epoxy plug less of a
reliability threat to the PTV barrel. On the other hand, the epoxy will have a
larger CTE than the epoxy, which could make things worse, except that the
partial fill near the MLB surface should make this not a real problem enhancer
either. So, my 5˘ says, that I do not think partial epoxy fills represent a
real reliability threat.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|