TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Universal Circuits - Buffalo <[log in to unmask]>
Date:
Tue, 16 Dec 1997 07:19:39 -0600
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Universal Circuits - Buffalo <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
        We have been laminating with single ply construction at our Buffalo
facility for three months now and have not experienced any problems. We
have recently started to laminate with single ply at our Maple Grove
facility and have run into a problem. I was wondering if anyone has come
across this same problem. What we are seeing is copper spots in the oxide
after lamination. We etched the foil off of several panels and to one
degree or another we have seen these spots. We ran several test lots with
the single ply 7628 high resin layup and our standard 1080/2116. The copper
spots did not show with the 1080/2116 layup. We are using Electrochemicals
oxide and we go into a post dip(reducer). Our laminate supplier seems to be
leaning toward the oxide as the problem. If anyone has experienced this
problem let me know.

Anthony Carfagna
Engineering Manager
Universal Circuits, Inc. - Buffalo

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2