Hi,
I guess you need to know where the solderballs originated from. Are you
referring to the solder balls generated from the wave-soldering process or
from the reflow soldering. It may be better to know the root causes, and
probably minimize it, rahter than brushing
Poh
=============================================================================
At 01:54 PM 12/11/97 +0200, Kiiski Jarmo KIISKJA wrote:
>Dear Techneters,
>
>In our production has arise a question about brushing solderballs off
>the boards with ESD-hand brush. The question is that would brushing
>degrade the realibility of the assembly by creaiting metallic traces on
>the soldermask or on the SMD-components.
>
>I would like hear about you experiences.
>
>Jarmo Kiiski
>Enermet Oy
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|