TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 10 Dec 1997 23:03:13 EST
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, JSSallo <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Organization:
AOL (http://www.aol.com)
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (20 lines)
There could be a variety of G 10 materials, just as there are a variety of FR
4.
You could have difunctional, multifunctional, etc. Tell your laminator what
you need and he can probably do similar Tg to FR 4.
J S Sallo
Sallo Consulting Services
760 346 6717

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2