TECHNET Archives

December 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Hong Yuen Electronics Ltd." <[log in to unmask]>
Date:
Tue, 9 Dec 1997 21:41:32 +1100
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Chi-man Chan <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Chi-man Chan <[log in to unmask]>
Parts/Attachments:
text/plain (48 lines)
There are three main reasons cause LISM under develop. They are:
1. Over track dry
2. Over exposure
3. Under develop

If you use a batch oven for track dry, I suggest you  check the temp.
distribution and air
circulation of your oven. Printed panels should be racked 1 cm (min.)
space. It will provide
a better air circulation. Reduce the temp. by 2 deg C if you still have
the problem.

Your exposure energy seems a bit too high for me. I usually set the
stepwedge solid 8-10
on copper.

You should also check the developing condition.

Spray pressure    > 2.0 bar
Soln. temp.          30-35 deg C
Developing time   > 1 min. (breakpoint ~10%)
Soda ash             0.8-1.2 %
Rinse pressure     > 1.0 bar
Rinse time            > 30 sec.
Rinse temp.         > 20 deg C

Mixed LISM should be used within 24 hrs and Printed panels should be
exposed/developed
within 24 hrs.

I hope the above information can help. Good Luck!

Best Regards,

Chan Chi Man

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2