Bev/Thomas ... I'm confused too ... Teflon has high surface resistivity --
unless of course it is highly filled with carbon (powder) or similar
conductive materials. What exactly is there about the Teflon that you want
to replace it?
At 01:06 PM 11/5/97 -0500, you wrote:
>THOMAS,
>Just being picky, but if it is a plastic then by definition it contains
>carbon. Perhpas there are silicone based boards with a CVD or PVD metal
>coating or a conductive ceramic that meet your needs, but it does sound
>rather novel to me!
>
>Bev Christian
>Nortel
>
>>----------
>>From: Lepsche, Thomas G (NM75)[SMTP:[log in to unmask]]
>>Sent: Wednesday, November 05, 1997 12:11 PM
>>To: [log in to unmask]
>>Subject: [TN] Teflon replacement
>>
>>Technetters,
>>
>>Does anyone know of a high temperature, conductive (low surface
>>resistively),
>>chemical resistant plastic (no carbon) that can be substituted for
>>Teflon.
>> Is there a company that specializes in this type of plastic?
>>
>> Thanks for your help!
>>Semper Fi
>>Tom
>>
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>>text in the body:
>>To subscribe: SUBSCRIBE TECHNET <your full name>
>>To unsubscribe: SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>>information.
>>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>>847-509-9700 ext.311
>>##############################################################
>>
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|