Howard
See IPC-D-275 table 3-1.
.00012" per volt on external layer with conformal coating.
.0001" per volt internal layer.
.001" per volt at high altitude without conformal coating.
.0002" per volt at 0- 10K feet exterior layer without conformal coating.

Rodney
my opinions are mine

\__________(*)__________/

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2