        We experienced some staining on the gold tips after the job passed
     through the OSP finishing. These are what happened:

     * Before going into OSP line, the gold tips looked perfectly normal.
     * After OSP, the first tip among the tips row was reddish in color,
     but all the other tips were OK.
     * The gold and nickel thickness were well within the sprcification.
     * The staining did not happened on other jobs.
     * The particular tip connection was intentionally cut off, then the
     board was run through OSP again. The same thing happened. This
     indicated that it wasn't any electrochemical effect.

     Can somebody give me some clue about this problem.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2