Lucy,
While at IBM (1982-1983) I qualified Water Soluble Tape. It works
extremely well with wave solder applications. You may search for my T#
51.0525. If you like I can supply this tape. Send me an email of your
application so that I can recommend the correct tape size or dot size.
##############################################################