TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 26 Nov 1997 16:15:14 +0100
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
From:
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset=US-ASCII; name="[TN]"
MIME-Version:
1.0
Parts/Attachments:
[TN] (20 lines)
Hello, Phil.
I use to try Kl/I2/H2O (4g/1g/40ml) plus Ammoniumpersulfate in the
proportions 1:1. Mix fresh every time.  And be careful with  no acids
into it. Keep locked and permit no others to play with it without
instructions. / If you want to etch the Tin part use HNO3 or FeCl3 in
different deionized water concentrations. Certainly, there are many
ohter ways. / Ingemar

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2