Something the company I work for has done, on occasion, has been to place a
'DAISY CHAIN' coupon on the waste area of our processed panel (we call it a
master). Basically, a series of the smallest hole on the board, with
alternating connections on the comp & ckt sides of the pcb (forces current
through the vias). Place an ohm/continuity meter on the start and end
points and check for a connection. If a failure is found it is very easy
to locate the offending hole, cross-section and determine a reason. Qty of
vias on the board vs qty of vias on the coupon must be evalutated (10000
vias, you don't want a 5 hole coupon.)
If a substantial problem exisits, try putting a DC coupon on the waste rail
of your array, will cost more but may be worth it...
JOE SENDZ.....
----------
> From: Bogdan Gaby <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Plating integrity in small vias
> Date: Monday, November 24, 1997 7:11 PM
>
> Hello,Technetters!
> Skipping the horror story,I have a question to printed circuit
> manufacturers:
> How do you ensure the integrity of the plating in small vias?
> We require the manufacturer's cross sections as a proof of test
> for our circuits.Very seldom,they contain small vias.
> But,anyway,the failures found recently in our line are in random places
> on the boards.
> Are there other tests on bare boards which can detect reliability
> problems ?
>
> Thank you
> Gaby
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|