Hi Brett,
I pulled out an old copy of MIL-S-13949. From what you have provided, I
believe the materials are described as follows:
FL-GB .062 - 13949/2 plastic sheet, laminated, metal clad, base
material GB, glass base, woven, majority polyfunctional expoy resin, hot
strenth rentention, copper-clad with thickness .062"
FL-GE .062 - 13949/3 plastic sheet, laminated, metal clad, base
material GE, glass base, woven, majority difunctional epoxy resin, general
purpose, copper-clad with thickness .062"
Hope this helps.
Steve Sauer
##############################################################