Try Buehler's Epo-Thin or Epo-Quik. We use these and don't have any
problem filling vias.
Bev Christian
Nortel
>----------
>From: Rogers, Lance M.[SMTP:[log in to unmask]]
>Sent: Monday, November 03, 1997 8:44 AM
>To: [log in to unmask]
>Subject: [TN] A better wetting compound for cross-sections?
>
> Hi Techneters.
>
> I am looking for a fast curing epoxy, that will wet holes 11.0
>mils or smaller. At present time we are using BUEHLER Sample Quick that
>sets in 5 minutes and is cured in ~ 10 minutes. The only problem we are
>having with this epoxy is that it has a very poor wettability of small
>holes. So when you go to polish these samples the holewalls have a
>tendency to collapse due to the lack of support in the hole.
> We used to use BUEHLER Epoxide with a cure time of about 2 to 3
>hours. This agent had fairly good wetting properties but unfortunately a
>little slow if you want to return results in a timely manner to the
>shop.
> Does anyone know of a compound out there that cures quickly and
>has a good wettability in 11.0 mils or smaller holes.
>
> Thank you
>
>
>Lance Rogers
>[log in to unmask]
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|