Technetters --
If anyone out there is encapsulating coomponents and/or assemblies in both
epoxy and silicones, are the areas where the encapsulation is done separated
from each other? If so, in what ways (ie different rooms, dedicated
cleaning lines, etc). If not, have you experienced any problems that might
have been eliminated by seperating the areas? We are trying to make an
informed decision as to how much physical separation is needed, if any.
These are not clean room operations, by the way. Thanks in advance for any
experiences.
Sheila Smith
Tracor Aerospace
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|