Sorry for asking, but why in the world would you want unfused tin/lead
on what I am presuming is a copper conductor. The tin will migrate into
the copper forming a tin-copper intermetallic layer very quickly; the
solderability of such a surface will be very poor. You can plate tin-nickel
or solder over nickel and have much better results, both for solderability
retention and for acting as a "lubricant" in the case of tin-nickel.
Perhaps you could elaborate as to what you are trying to acheive.
Regards,
Fred J.
>>> Aric J Parr <[log in to unmask]> 11/05/97
01:50pm >>>
I am trying to find a specification for plating tin/lead on some
parts. I do not want it fused.
I haven't found an IPC spec for this.
Can anyone help me?
Thanks,
Aric Parr
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|