If you have are "left with a bare lead with no solder on it", that means you
never had a solder joint in the first place. You clearly had no wetting, for
whatever reason. Corrosion (after soldering) is not the problem.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
23 Gunther Street In December: 7 Jasmine
Run
Mendham, NJ 07945 Ormond Beach, FL 32174 USA
Phone & Fax: 973-543-2747 Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|