TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset=US-ASCII
Sender:
Subject:
From:
Larry Crane <[log in to unmask]>
Date:
Tue, 25 Nov 1997 07:41:22 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Larry Crane <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
Responding to the comment by Graham about solder mask doing a temperary
job.  This was probably true for the origonal use.  However requirements
have far surpased the origonal description and the solder mask does a
permanent job protecting the FR-4 and copper circuitry.  UL lists Solder
masks as permanent polymer coatings.  Conformal coating is used to protect
leads and devices.  Because of the sequence of application one cannot due
the job of the other.

As far as epoxy resins being hydroscopic this is both true and false.
There are many types of epoxy resins and curetives and depending on the
selection the cured epoxy resin can either be hygroscopic or not.  Solder
Masks are tested to very high levels of moisture and do quite well.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2