An Ionograph is a very recommendable piece of equipment, if that is the tool
you are referring to.
Contaminants which do not wash off well can cause reliability shorts if they
are conductive. Ionograph testing is a good way to find them.
Also, poor drying of the boards can cause SnPb oxides to cause shorts across a
board. I have seen well washed, but poorly dried boards develop dendritic
growth shorts from the SnPb of the solder joints.
Jim Herard
KBL, Product Quality Engineering
IBM Microelectronics Endicott
t/l 857-7026
[log in to unmask] on 11-13-97 05:26:03 PM
Please respond to [log in to unmask] @ internet
To: [log in to unmask] @ internet
cc:
Subject: [TN] Do we really need ionic contamination measurement equip
SMT/Wave Process Expert,
If the conductivity of the DI water of wash machine is maintained along with
good maintenance of the wash machine, do we still feel that it is always or
must to have ionic contamination measurement equipment like one of that
Alphametal makes?
I am really interested in pros and cons of having such system from need
point of view rather than sales pitch (to show to prospective customers).
Re,
Ken patel
______________________________________________________
Ken Patel Phone: (408) 490-6804
575 Cottonwood Dr. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe:
SIGNOFF TECHNET ##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information. For the technical support contact Dmitriy Sklyar at [log in to unmask]
or 847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|