Post again for advise on this issue.
> ----------
> From: Dhawan, Ashok
> Sent: September 25, 1997 7:30 AM
> To: 'IPC TechNet'
> Subject: lead trimming
>
> Of and on we come across field failure on lead trimming--the annular
> ring is damaged or scratched.
>
> The initial analysis showed that it could be due to trimming tool head
> being flush head type.It could be trainning issue.
>
> What is norm on trimming cutter head type and what is kind of approach
> to trim the lead after wave ??
> Is there automated trimmer tools for soldered boards??
> I know trimming before wave or prep components is very cubersome
> process.
>
> How you guys are handling such an issue?
>
>
> [log in to unmask]
>
>
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|