I have seen similar problem and we simply stop our SMT line and send fabs
back to fab house for resurfacing. We were able to run without problem
second time so your half answer is that yes fab house can fix it.
re, ken patel
At 04:22 PM 10/29/97 -0400, Jim Marsico 516-595-5879 wrote:
>We've been receiving some boards from our supplier which exhibit dewetting on
>the surface mount pads. The solder on the pads is much thicker on one end and
>the balance (about 75%) is very thin. We have had some non-wetting on the thin
>portions during assembly. The boards are HASLed, obviously the solder is blown
>off in the direction of the thicker solder areas. My question is this, what is
>the fabricator doing wrong, and can these boards be reworked?
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
>
______________________________________________________
Ken Patel Phone: (408) 490-6804
575 Cottonwood Dr. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|