In terms of cost, our MRP system "charges" $ 0.25/square inch of surface
gold plated per 25 millionths of an inch thickness of gold. There is
presently no distinction in cost for the Type 2 versus the Type 3 gold. As
an example, a housing cover with 12 square inches of surface to be plated
would cost $ 3.00 for the "standard" gold/nickel on aluminum [200 millionths
EN, 25 microinches gold]. This is the minimum charge if gold plating is
applied.
At 01:46 AM 10/26/97 -0700, you wrote:
>Can anyone share with me what the cost differiental (percentages are fine)
>between heavy gold plating (25 microinches) versus flash gold (5-6
>microinches)? I am trying to evaluate the cost benefit for changing to
>flash gold. How much of the board cost is allocated to gold plating costs
>(again, percentages are fine)? What is percentage of the board cost for 25
>microinches of gold? Percentage for gold flash? Any comments would be
>truly appreciated.
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|