dear ron,
the problem can be improper stripping of Tin-lead or the loading of
electroless nickel bath may be less . look into these areas.
radhakrishnan
indal electronics limited
At 01:02 PM 10/15/97 -0700, you wrote:
>PWB manufacturers:
>Has anyone seen the phenomonen of exposed copper SMT pads after
>immersion NiAu. To further complicate this issue, any pad (via or SMT)
>that is tied to this pad in a net also does not get plated. This condition
>does not occur on every panel within the rack. One panel will have it,
>while the adjacent panel does not.
>Are we looking at a static charge on the panel that keeps certain nets
>from plating?
>Any ideas on what's causing this would be appreciated.
>
>Thank you
>Ron Hayashi
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
>
With Best Regards
Your's truly,
Anthony Balraj
---------------------ooo---------ooo----------------------
INDAL ELECTRONICS LIMITED.
12/A, Industrial Area,
Nanjangud - 571 301.
Email:[log in to unmask] Karnataka, INDIA.
Ph:(+91-8221)26618,26619,26375,26584 Fax:(+91-8221)26641
---------------------ooo---------ooo----------------------
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|