Only one way I know to eliminate gold slivers and that is to etch first, electroless gold after.
Ed Cosper
----------
From: Art Shuler[SMTP:[log in to unmask]]
Sent: Tuesday, October 07, 1997 12:00 PM
To: [log in to unmask]
Subject: [TECHNET] Gold Slivers
Does anyone know of a way to completely eliminate gold slivers on a PWB
which is manufactured using a selective gold process? We realize due to
the etch factor, that there will be a 1.4 mil outgrowth when etching 1
oz. copper cladded material.
Mil-P-55110 recognizes that outgrowth will be present on conductors
plated with metals other than solder, but our customer cannot tolerate
slivering. We've tried brushing them off with a brass wire brush, but
this seems to aggravate the problem.
Any input would be greatly appreciated.
Thank you
Art
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|