At 09:36 AM 10/1/97 E, you wrote:
>Regarding Plastic Parts:
>
>
>When a part is identified as having an allowable exposure time of 48 hrs...
>
>1) Can I expose it for 24 hours, seal it in a moisture barrier bag for some
>extended period of time, and then expose it for another 24 hours? In other
>words, is it safe to assume that this is CUMULATIVE exposure time?
According to IPC, yes it is cumulative (IPC-SM-786)
>
>
>
>
>2) If you open a bag just to pull a couple of parts, and then reseal the bag
>(minutes of exposure) does that present any problems?
If it is open for less than 30 min., it does not present a problem (IPC again)
>
>
>
>
>For those who respond, please clarify whether this is your internal
>procedure, or if it is documented in IPC, or elsewhere.
>
>
>
>Thanks,
>
>Mike
>[log in to unmask]
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
>
Marie-Josée Lambert
------------------------------
Ingénieure de procédés
Tél.: (514) 969-6000 Ext.7578
E-Mail: [log in to unmask]
------------------------------
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|