Hi Steve,
From prior experience:
1. If your people are going to do any splicing
of fiber-optic cable, make sure they do it
with gloves over a barrel specifically for
the waste. The sheared pieces of fiberglass
are worse than splinters.
2. Make sure that handling the cable ensures
the ends are protected from handling and
dirt.
Little rubber caps should come with
the cables (if pre-assembled) to cover the
ends. Also, the caps may indicate what
kind of "cut" was done to the end of the
cable - straight or angled. Some fiber
is cut straight across the cable for a
flat connection into what it's being
plugged into. Others have an "angled"
cut. The two are obviously incompatible.
A cleaning solvent and q-tips are for cleaning
the dirt. I believe some solvents will leave
a residue, so check on this. It's been a while
for me. Good practice is to clean the fiber EVERY
time a connection is made.
Regards, Doug
----------
> From: Steve Mikell <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TECHNET] Fiberoptic device handling
> Date: Wednesday, October 08, 1997 9:36 AM
>
> Today's mission is to locate any special procedures regarding the
handling
> or storage of fiberoptic cable or devices. We are obviously not going to
> immerse the connector in any cleaning solutions, but we are interested in
> any special problems which fellow technetters have encountered. Thanks
for
> any tips.
>
> Steve Mikell
> Industrial Engineering
> SCI Systems Plant 13
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|