Typically FR-4 has a glass transition temperature of about 140
Celsius. It would not be wise to be in an operating temperature above
this value. All material manufacturers will have there own specific
material specifications. Some of the manufacturers are GE, Allied
Signal, Hitachi, Nanya, Toshiba just to name a few.
A good book with all these specifications is the World Metal Clad
Laminates Data Book. The Mitsubishi Rayon Group, Publisher: MCR
Techno Research Inc. Japan Phone # 81-44-900-7580 Fax: 81-44-900-7582.