At 11:43 AM 10/30/97 -0500, you wrote:
>Our customers have found that a good alkaline cleaner, used as hot as
>possible, and as long as possible, perhaps even used as an electrocleaner, to
>shorten the process time, is the key, after that any weak acid solution,
>Sulfuric is great, then rinse and plate.
>
>I can give you more information directly, or contact Dynavest, or their
>subsidiary Comacraft, with offices in Penang, KL, Manilla, and Singapore.
>
>Rudy Sedlak
>RD Chemical Company
To : Rudy sedlak
Thanks a lot for your input .I have tried that before but it do not work .
Please elaborate further on sulphuric acid , operating % , temperature , any
ppm of Fe or Ni the bath can tolerate because sulphuric acid will attack
alloy42
and gives rise to Fe3+ and a yellowish brown discoloration to the alloy42 .
Please advise .Thanks .
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|