Subject: | |
From: | |
Reply To: | TechNet Mail Forum. |
Date: | Fri, 3 Oct 1997 10:12:47 -0400 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
John
Your paper sounds interesting, I would be interested in a copy. It may
also help me with my current issue, cracking glass bodied diodes...
Thanks!
regards,
Graham Collins
Litton Systems Limited, Atlantic Division
(902) 873-2000 ext 215
> -----Original Message-----
> From: john maxwell [SMTP:[log in to unmask]]
> Sent: Thursday, October 02, 1997 9:20 PM
> To: [log in to unmask]
> Subject: Re: [TECHNET] [T] Cracking of 1206 components
>
> >I do not know which 'thermal shock issue' you investigated; heating
> too fast
> >or cooling too fast? Chip components, unless already defective, do
> not crack
> >on fast heating, but can do so on fast cooling. That can happen in
> >combination with pad designs that allow exessively large solder
> fillets. When
> >these large solder volumes cool, they shrink at ~25 ppm/C and the
> ceramic
> >chip components at only ~6 ppm/C. When you cool too fast the solder
> can not
> >creep fast enough to relax the stresses and component cracking can
> result.
> >
> >Werner Engelmaier
>
> To those that have experienced ceramic capacitor cracking.
>
> First, barium titanate capacitors have coefficients of expansion
> ranging
> from about 9 ppm/degree C for NPO glassy ceramics to about 11-12
> ppm/degree
> C for X7R and Z5U type materials. Alumina based chips like resistors
> have a
> CTE of approximately 6 ppm/degree C. With the rare exception of very
> large
> solder joints rapid cooling has not been a problem in capacitor
> cracking.
> Large fillet size coupled with excessive glass diffusion during
> termination
> firing is the usual culprit.
>
> The crack shape tells all and was documented in a paper I wrote in
> 1987
> while working for AVX which was titled "Cracks: The Hidden Defect". It
> was
> later made into an application note and may still be available at
> their web
> site located at avxcorp.com. If not contact me off the forum and I
> will
> send you a copy. Capacitor cracking can have many surprising sources
> so
> check the crack signature first to get a better idea on where to look
> for
> the root cause.
>
> Regards,
>
>
> John Maxwell
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|