TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Wed, 29 Oct 1997 21:08:36 +1100
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Nicholas Kane <[log in to unmask]>
Subject:
From:
Nicholas Kane <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (93 lines)
Could you perhaps fax me this article also?

Thankyou

Nicholas Kane
Axion Australasia
651 Canterbury Road
Surrey Hills
Victoria
Australia
fax 613 9899 3811

At 11:24 28/10/97 -0500, you wrote:
>Marie:
>
>We do not supply anything in waste treatment, but as a chemistry supplier, we
>are intimately involved in the issue.   I advise you that the BEST thing that
>you can do to ease the issue, and cut costs is to separate your wastes, and
>treat them in different ways.
>
>The presumption is that the only issues that you have in your waste water are
>pH and dissolved heavy metals.
>
>Most of the time you can separate your waste streams into the following
>categories:
>
>1. Chelated, low, to neglible metal (rinses from resist strippers, alkaline
>cleaners, etc.)
>2.  Chelated, high metal, (Electroless Copper rinse, and bailout, ammoniacal
>etch rinse)
>3. Non-Chelated, high metal (microetch rinse, electrolytic plating rinse,
>etc.)
>
>On the first category, simple pH adjustment may be all that is required, do
>this, and put it down the drain, if the metal is low enough, do not allow the
>chelates to mix with category three, or you jack the cost of treatment to the
>sky.
>
>Category three can best be treated by pH adjustment, and precipitation of
>metal sludge.
>Cheap and simple.
>
>Category two is the big expense, and if you mix all your wastes, all the
>waste becomes category two waste.   This must be treated by ion exchange, or
>precipitation with special chemicals, like sulfides, or weird expensive
>organics, to remove the metals from the chelates.
>
>This is pretty general stuff, but it is very often overlooked as a powerful
>tool to assist and cut costs in waste treatment.
>
>If I can be of more assistance, contact me off line.
>
>Incidently, if you want to send me your fax number, I have an article on
>chelates and waste treatment that you might find interesting.
>
>Best regards,
>
>Rudy Sedlak
>RD Chemical Company
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
>
Nicholas Kane
Axion Australasia
Suite 3, 651 Canterbury Road
Surrey Hills
Victoria 3127 Australia

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2