Good point, however, the solder joint I am concerned with is attaching a
Kovar connector into an aluminum housing -- no FR4 is involved. Still the
"new" solder compound being created could be a concern. Sheila @ TRACOR AES
At 01:28 PM 10/23/97 -0400, you wrote:
>Dave, Sheila,
>Although soldering irons can certainly melt the 95/5 solder isn't there
>an increased risk of damage to the board because of the application of
>the higher temperature to the FR-4?
>Bev Christian
>Nortel
>[log in to unmask]
>
>>----------
>>From: David D Hillman[SMTP:[log in to unmask]]
>>Sent: Thursday, October 23, 1997 11:59 AM
>>To: [log in to unmask]
>>Subject: Re: [TN] [TECHNET] ASSY: Solder compatibility
>>
>>Hi Sheila - a question - do you know that the voids are detrimental to
>>solder joint reliability? Also mixing of 95/5 with Sn62 is probably not
>>going to give you an intermetallic issue but you will probably get a
>>reeeaallly neat solder joint composition which will be very hard to predict
>>any type of properities data or even a simple melting point. If you must do
>>touchup why not use 95/5 as the touchup alloy? Soldering irons can melt
>>that alloy. Good Luck.
>>
>>Dave Hillman
>>Rockwell Collins
>>[log in to unmask]
>>
>>
>>
>>
>>
>>[log in to unmask] on 10/21/97 10:05:36 AM
>>
>>Please respond to [log in to unmask]; Please respond to [log in to unmask]
>>
>>To: [log in to unmask]
>>cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
>>Subject: [TECHNET] ASSY: Solder compatibility
>>
>>
>>
>>
>>Hello TechNet ..
>>Does anyone have any experience with possible intermetallics formation if I
>>use Sn62Pb362Ag to touchup voids in a Vapor phase reflowed Sn95Sb5 solder
>>joint ??? Especially after 100 temp cycles from -55C to 120C? Thanks for
>>any help!
>>Sheila Smith, Tracor AES
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>>text in the body:
>>To subscribe: SUBSCRIBE TECHNET <your full name>
>>To unsubscribe: SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>>additional information.
>>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>>847-509-9700 ext.311
>>##############################################################
>>
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>>text in the body:
>>To subscribe: SUBSCRIBE TECHNET <your full name>
>>To unsubscribe: SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>>information.
>>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>>847-509-9700 ext.311
>>##############################################################
>>
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|