TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"NCPPaul @aol.com" <[log in to unmask]>
Date:
Fri, 24 Oct 1997 07:29:10 -0400
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (29 lines)
All the responses have included just chemical regen options, but ORP can be
maintained with electricity. FSL manufactures an Electroletically
Regenaration Unit that maintains ORP without adding in needless water (H2O2).
 The capitol investment is high but the ROI is quick, if all cost considered.
With chemical regen system costs would include the chemistries, HCL and
Chlorine/H2O2/or Sodium Chlorite. The amount of HCL used in any system will
depend on the type of Oxidizer.  The waste cost is a factor, in house
treatment or off sight treatments. With the FSL unit the regen cells plate
out almost pure copper that can be sold, with no waste treatment discharge.
HCl is used to maintain Normality but at a much lower consumption rate than
the chemical oxidizers.  I have seen two diffirent insallation in the New
England area that has been up and running.
I do not represent FSL. I'm just giving other alternatives for Cupric
Chloride Regen.
I am unsure of any down side to this system. If anyone has any input please
feel free to comment.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2