TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Greg Finlay <[log in to unmask]>
Date:
Thu, 23 Oct 1997 10:23:56 -0400
MIME-Version:
1.0
X-To:
Jan Vercammen <[log in to unmask]>
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Greg Finlay <[log in to unmask]>
Parts/Attachments:
text/plain (64 lines)
Compositech Cores  are 60% E-glass. Their web address is
http://www.compositechltd.com and has some of the info your looking for.


        -----Original Message-----
        From:   Jan Vercammen [SMTP:[log in to unmask]]
        Sent:   Thursday, October 23, 1997 9:32 AM
        To:     [log in to unmask]
        Subject:        [TN] dielectric data E-glass fiber

        hello,

        I am interested in the dielectric constant and dielectic loss
factor of
        E-glass type fibers in function of frequency. I have searched
the web and
        literature for data on this subject, but I have only found
conflicting
        data.

        My interest is purely for +50MHz frequencies, the E-glass has a
chemical
        composition as defined in IPC-EG-140: B2O3 (5-10%), CaO
(16-25%), Al2O3 (12-16%,
        SiO2 (52-56%), MgO (<5%),Na+K2 (0-2%), TiO2 (0-0.8%), Fe2O3
(<0.4%), F2 (<1%)


        Your help is kindly appreciated. Data, references, brochures,
..., everything
        is welcome.


        Jan Vercammen
        Agfa
        [log in to unmask]

        ##############################################################
        TechNet Mail List provided as a free service by IPC using
LISTSERV 1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask]
with following text in the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm)
for additional information.
        For the technical support contact Dmitriy Sklyar at
[log in to unmask] or 847-509-9700 ext.311
        ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2