Fellow Technetters,
At present we use a screenable laquer from Lackwerke Peters
(Werner Peters SD 2955) to cover inboard Ni/Au (hardgold)
contacts/connectors during horizontal hot air levelling.
In a few months however we are not allowed to use the fluid to strip
this laquer anymore, due to enviromental reasons.
We have tried peelable solderresists but these are not 100 %
resistant to the pressure during horizontal hot air levelling resulting
in P/Sn particles on the Ni/Au contacts.
Manual taping is also no option volumewise.
# Which materials/processes are available for manufacturers which
use horizintal HASL to cover, in medium/high volume, inboard
Ni/Au contacts before HASL?
Any thoughts on the subject or any other alternatives would be
appreciated.
Thanks,
Rob van Pol
MOMMERS PRINT SERVICE B.V.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|