Hello Chris,
We have two 10 years old Schering (Now Atotech) plating lines that had
been upgraded with the latest Atotech control system (DYNATRON H) in
April 97.
Along with the upgrade, we received a special software to help us
develop our own timeway diagram. This special software generates all the
codes necessary by itself so we don't have to write a line of code to
implement a timeway change but I believe you may use the same software
to generate your timeway for a different plating line since it makes the
job easier to manage all transporter moves and dwell time in a WYSIWYG
fashion.
There is also GEOTRONICS that provides such timeway simulator software
but I have no experience with this one.
Here are the coordinates for both companies;
ATOTECH
Kurt W. Astor
Atotech Deutschland GmbH (Germany)
Project manager
Tel: (09128) 71-386
Fax: (09128) 71-246
GEOTRONICS
Greg Arneson
Sales / Marketing Manager Dynamic Positioning System
Geotronics of North America, inc
Tel: (847) 854-2489
Fax: (847) 854-5975
Regards,
Charles Desroches
Technical Advisor
Circo Craft
[log in to unmask]
> ----------
> From: Chris Ford[SMTP:[log in to unmask]]
> Reply To: TechNet Mail Forum.;Chris Ford
> Sent: Wednesday, October 15, 1997 11:02 AM
> To: [log in to unmask]
> Subject: [TECHNET] Time Way Software
>
> Good Day All:
>
> We are looking to obtain software to be able to program our own
> time-ways for automatic plating processes. Could anyone out there
> furnish us with names and phone numbers of companies which publish
> this type of software?
>
> Thank You!
>
> Brad Mulhern
> Plant Engineer
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|