Gee Bill, sounds mighty strange to me! When we've had moisture related
failures in temp cycling it was attributable to corrosion/conductive paths
under the conformal coating caused by incomplete flux residue removal prior
to coating boards. Is there a possiblity that your urethane coating is not
completely cured or that the boards weren't baked to drive off residual
moisture prior to coating?
Sheila Smith, Tracor AES
At 11:19 AM 10/17/97 -0400, you wrote:
>
> We are experiencing temperature cycle (-37C to 55C) test
>failures on mixed technology (thru-hole one side, SMT other side) PWB
>assemblies coated with Polyurethane per Mil-I-46058. The same assemblies
>pass static temperature testing at the low, ambient and high points of
>the temperature range. Uncoated assemblies will pass the temperature
>cycle test. It is suspected that small bubbles in the conformal coating
>(within allowable size per specification criteria) are accumulating
>condensation during temperature transitions, causing bridging between
>conductive surfaces on the SMT components. Has anyone experienced
>similar problems?
>
>
>Bill
>
>Bill Bromley
>Lead Designer
>Lucas Aerospace PSA
>MailStop D960
>777 Lena Dr.
>Aurora OH 44202-8025 USA
>voice: 330-995-1000 ex 3092
>email: [log in to unmask]
>
>
>Attachment Converted: C:\EUDMAIL\TECHNETA
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|