TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
Dan Babcock <[log in to unmask]>
Date:
Wed, 15 Oct 1997 16:56:43 MDT
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Dan Babcock <[log in to unmask]>
Parts/Attachments:
text/plain (44 lines)
Hi Christina -- The paper entitled 'Effect Of Au On The Reliability Of
Fine Pitch Surface Mount Solder Joints" from the 1991 SMI Proceedings may
provide some helpful information. I can Fax a copy if you'd like.

Dan Babcock
Sr. Engineer
Maxtor Corp
[log in to unmask]

>Subject: Brittle Solder Joints
>
>Hello,
>
>I am looking for some information either from experience or papers on
>what causes brittle solder joints.  We have immersion gold over nickel
>and use eutectic solder paste. Board material is high-temp FR4.   I
>would like to know:
>
>1.  How many heat cycles a solder joint will tolerate without becoming
>brittle.  Is there a temp that a solder joint becomes brittle and the
>crystalline structure changes (as in steel tempering)?
>2.  What would be the definition of a heat cycle (would it be reaching
>183 C or something else)?
>3.  What is a safe temp to have boards at  during a stress testing..
>
>any information or a contact to find information would be greatly
>appreciated.
>Thanks in advance for your help,
>
>Christina Piasky ([log in to unmask])
>Sequent Computer Systems

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2