TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Ron Hayashi <[log in to unmask]>
Date:
Wed, 15 Oct 1997 13:02:57 -0700
Content-Type:
text/plain
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Ron Hayashi <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
PWB manufacturers:
Has anyone seen the phenomonen of exposed copper SMT pads after
immersion NiAu. To further complicate this issue, any pad (via or SMT)
that is tied to this pad in a net also does not get plated. This condition
does not occur on every panel within the rack. One panel will have it,
while the adjacent panel does not.
Are we looking at a static charge on the panel that keeps certain nets
from plating?
Any ideas on what's causing this would be appreciated.

Thank you
Ron Hayashi

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2