TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Ron Hayashi <[log in to unmask]>
Date:
Wed, 1 Oct 1997 13:42:41 -0700
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=ISO-8859-7
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Ron Hayashi <[log in to unmask]>
Parts/Attachments:
text/plain (14 lines)
I'm not too sure if gold embrittlement would even be an issue with the thicknesses offered by Immersion gold plating.  2 to 6 ì inches should not cause any issues.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2