TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Lang, Michael" <[log in to unmask]>
Date:
Mon, 13 Oct 1997 16:52:00 E
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, "Lang, Michael" <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
I have asked several questions regarding plastic parts with good results,
but still have one issue.

Throughout IPC-SM-786A there is reference to baking out plastic parts at 40C
and <5%RH.

HOW?


Who has the equipment to bake under these conditions?   I assume you need a
special oven to keep the humidity low...  A regular oven running in a
standard ESD safe environment will not have such a low RH inside...


Thanks,

Michael Lang
[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2